#121 OFFLINE   hubel458

hubel458

  • Group:Members*
  • Posts: 161
  • Joined: Jun. 25 2009
  • Location:Brinton, MI


Posted May. 10 2018 - 11:22 PM

Here is sectioned 585  HE case in the middle, we first  made from
 
another case, years ago  before we had factory run of brass and
 
 it had perfect thickness on the sides and inside corrner.
 
We could fire them many times without sides thinning..
 
First case is  factory run of  our 585 HE,  3rd  is case that is too 
 
thick of  sides and sticks at high pressures..
 
goodone.jpg 
 
Pic of  our factory run cases necked down to 375 and fired 4 times
 
at high pressure on the right,  with unfired case on the left. 
 
Our case is not perfect but does work...Ed
 